For oil based paints slow drying is a benefit since this allows the paint to.
Raw linseed oil for vinily siding.
Do you know what the difference is between boiled linseed oil and raw.
Cabot 140 007 semi transparent deck siding low voc stain gallon redwood.
Raw linseed oil dries very slowly taking weeks to fully cure.
Raw vs processed linseed oil.
The raw one does not dry.
The difference is that the boiled linseed oil is the only one that dries.
Store linseed oil only in metal containers and keep the drying furniture away from any heat sources.
Was she using boiled or was she using raw linseed oil.
Slow drying is a mixed blessing.
Keep any rags or papers you use to apply the oil in a metal container filled with water.
Restoring vinyl siding with linseed oil.
And so for a siding sealing material for an exterior finish you use boiled linseed oil.
The primary trouble in using linseed oil is that raw linseed oil takes a long time to cure up to two weeks in a dry well ventilated area and ultimately a couple of months if it is applied to surfaces that are exposed to extreme heat cold or high humidity.
Raw linseed oil can take up to a week to dry but the drying time can be significantly reduced by oxidizing it or adding metallic thinners a process known as boiling.
You should limit its use to the insides of wood gutters chopping blocks sawhorses and other items exposed to the elements where drying time is not a consideration.
The bottom line is that pure linseed oil can be very difficult to work with particularly in a case where it is a wood floor or deck.